WIRE COMPOSITION:
C Mn Si Cr Ni PSAl
0.17 0.52 0.34 0.02 0.02 0.012 0.003 1.42
TYPICAL MECHANICAL PROPERTIES OF DEPOSITED METAL
Tensile Strength, Mpa598
Yield Point, Mpa 442
Elongation, % 24
SIZE OF WIRE:
Diameter 1.2mm 1.6mm
Weight 1KG 5KG 15KG
PACKAGING
Plastic spool D200 D270 D300